Effectiveness and safety of bleaching agents on lithium disilicate glass ceramics

View through CrossRef
Background. Aesthetic expectations have increased the use of aesthetic materials in dentistry. Lithium disilicates are frequently used materials for these expectations. Bleaching is another method used to provide aesthetics. Bleaching processes on restorative materials are not fully known. This study investigated the effect of at-home and in-office bleaching methods on the color change, surface roughness, and topography of lithium disilicate glass-ceramic materials produced with two different techniques and subjected to different polishing procedures. Methods. A total of 144 disc-shaped pressed and computer-aided design (CAD) lithium disilicate glass-ceramic specimens were randomly divided into four groups. Glazing and three different chair-side polishing procedures were performed. The specimens in each group were randomly divided into two groups and subjected to at-home and in-office bleaching processes (n=9). The home bleaching process was repeated with 16% carbamide peroxide agent for six hours for seven days, while the in-office bleaching process was applied with 40% hydrogen peroxide agent for two sessions of 20 minutes. After the bleaching processes, the final color and surface roughness experiments of the specimens were carried out, and the results were recorded. ANOVA and Tukey multiple comparison tests were used FOR the statistical analysis of the data (α=0.05). Results. The material*polish*bleaching, polish*bleaching, material*bleaching, and material*polishing interactions were not statistically significant regarding color and roughness changes of both specimens (P>0.05). Conclusion. Both bleaching processes can be safely applied to lithium disilicate glass-ceramic materials.
Title: Effectiveness and safety of bleaching agents on lithium disilicate glass ceramics
Description:
Background.
Aesthetic expectations have increased the use of aesthetic materials in dentistry.
Lithium disilicates are frequently used materials for these expectations.
Bleaching is another method used to provide aesthetics.
Bleaching processes on restorative materials are not fully known.
This study investigated the effect of at-home and in-office bleaching methods on the color change, surface roughness, and topography of lithium disilicate glass-ceramic materials produced with two different techniques and subjected to different polishing procedures.
Methods.
A total of 144 disc-shaped pressed and computer-aided design (CAD) lithium disilicate glass-ceramic specimens were randomly divided into four groups.
Glazing and three different chair-side polishing procedures were performed.
The specimens in each group were randomly divided into two groups and subjected to at-home and in-office bleaching processes (n=9).
The home bleaching process was repeated with 16% carbamide peroxide agent for six hours for seven days, while the in-office bleaching process was applied with 40% hydrogen peroxide agent for two sessions of 20 minutes.
After the bleaching processes, the final color and surface roughness experiments of the specimens were carried out, and the results were recorded.
ANOVA and Tukey multiple comparison tests were used FOR the statistical analysis of the data (α=0.
05).
Results.
The material*polish*bleaching, polish*bleaching, material*bleaching, and material*polishing interactions were not statistically significant regarding color and roughness changes of both specimens (P>0.
05).
Conclusion.
Both bleaching processes can be safely applied to lithium disilicate glass-ceramic materials.

Related Results

Marginal Fit Comparison of CAD/CAM Crowns Milled from Two Different Materials
Marginal Fit Comparison of CAD/CAM Crowns Milled from Two Different Materials
AbstractPurposeTo evaluate the marginal fit of CAD/CAM copings milled from hybrid ceramic (Vita Enamic) blocks and lithium disilicate (IPS e.max CAD) blocks, and to evaluate the ef...
Unveiling the third dimension of glass
Unveiling the third dimension of glass
Glass as a material has always fascinated architects. Its inherent transparency has given us the ability to create diaphanous barriers between the interior and the exterior that al...
Clinical observation of two different resin cements on lithium disilicate glass-ceramic veneer
Clinical observation of two different resin cements on lithium disilicate glass-ceramic veneer
Objective: To assess the bonding effect of two resin cement on lithium disilicate glass ceramic veneer.Method: The study was conducted at the Medical School of Nanjing University, ...
A preliminary study of skin bleaching and factors associated with skin bleaching among women living in Zimbabwe
A preliminary study of skin bleaching and factors associated with skin bleaching among women living in Zimbabwe
Background: Skin bleaching was reported to be commonly practiced among women and Africa was reported to be one of the most affected yet the subject is not given much attention in p...
Roles of electrostatic interactions in the peroxide systems for bleaching of cotton fiber
Roles of electrostatic interactions in the peroxide systems for bleaching of cotton fiber
Abstract The industrial bleaching of cotton fiber is often carried out in an aqueous solution of hydrogen peroxide (H2O2) with the addition of sodium hydroxide (NaOH) at a ...
In vitro Comparison of the Microhardness of Lithium Disilicate and Monolithic and Multilayered Fixed Prosthodontic Materials
In vitro Comparison of the Microhardness of Lithium Disilicate and Monolithic and Multilayered Fixed Prosthodontic Materials
Micro-hardness is a fundamental property of prosthodontic restorative materials, as it affects their resistance to surface deformation, wear, and long-term clinical performance. Th...
Fracture resistance and mode of failure of modified Polyether-ether-ketone versus lithium disilicate endocrowns
Fracture resistance and mode of failure of modified Polyether-ether-ketone versus lithium disilicate endocrowns
Abstract Purpose The current study aimed to compare modified Polyether-ether-ketone's fracture resistance and failure mode versus lithium disilicate...