Workability and Flexural Strength of Recycled Aggregate Concrete with Steel Fibers
View through CrossRef
This study examined how concrete workability and flexural strength are affected by steel fibers and recycled aggregates. Steel fibers were used in doses between 1-5%, with an increment of 0.5%, and 50% of the natural coarse aggregates were replaced by recycled. Two mixes of conventional and recycled aggregate concrete without steel fibers were used as control mixes. Concrete mixes were prepared using 1:2:4 and 0.45 water-to-cement ratios. Workability was determined using the slump cone. Three prism specimens sized 500×100×100mm were prepared for each batch and cured for 28 days in potable water. After curing, the specimens were air-dried in the laboratory and tested to evaluate their flexural strength under two-point loading. The load and deflection were monitored at regular intervals until failure. A comparison of results with control mixes showed that as the percentage of steel fiber increased, flexural strength increased by 69% and deflection decreased by 66%. The use of steel fibers improved the flexural strength of the recycled aggregate concrete by 59%.
Engineering, Technology & Applied Science Research
Title: Workability and Flexural Strength of Recycled Aggregate Concrete with Steel Fibers
Description:
This study examined how concrete workability and flexural strength are affected by steel fibers and recycled aggregates.
Steel fibers were used in doses between 1-5%, with an increment of 0.
5%, and 50% of the natural coarse aggregates were replaced by recycled.
Two mixes of conventional and recycled aggregate concrete without steel fibers were used as control mixes.
Concrete mixes were prepared using 1:2:4 and 0.
45 water-to-cement ratios.
Workability was determined using the slump cone.
Three prism specimens sized 500×100×100mm were prepared for each batch and cured for 28 days in potable water.
After curing, the specimens were air-dried in the laboratory and tested to evaluate their flexural strength under two-point loading.
The load and deflection were monitored at regular intervals until failure.
A comparison of results with control mixes showed that as the percentage of steel fiber increased, flexural strength increased by 69% and deflection decreased by 66%.
The use of steel fibers improved the flexural strength of the recycled aggregate concrete by 59%.
Related Results
Mix Design Recycled Aggregate Pervious Concrete and the Influence on Pavement Property
Mix Design Recycled Aggregate Pervious Concrete and the Influence on Pavement Property
Abstract
This paper prepared recycled aggregate pervious concrete by replacing natural aggregate with 100% volume of waste concrete. We carried out experiments to st...
Microstructure of concrete prepared with construction recycled aggregates
Microstructure of concrete prepared with construction recycled aggregates
Conservation of natural resources, shortage of waste land and the high cost associated to treatment prior to disposal are driving growing interest in the recycling of construction ...
Experimental Study of Compressive Properties and Environmental Impact of Recycled Aggregate
Experimental Study of Compressive Properties and Environmental Impact of Recycled Aggregate
As the main component of fiber-reinforced recycled aggregate concrete, the properties of recycled aggregate determine whether recycled aggregate concrete can be used in engineering...
Influence of fly ash and basalt fibers on the properties of recycled pervious concrete
Influence of fly ash and basalt fibers on the properties of recycled pervious concrete
As an environmentally friendly building material, recycled pervious
concrete can not only alleviate the increasingly severe urban flooding
and heat island effect, but also realize ...
Eurocode Shear Design of Coarse Recycled Aggregate Concrete: Reliability Analysis and Partial Factor Calibration
Eurocode Shear Design of Coarse Recycled Aggregate Concrete: Reliability Analysis and Partial Factor Calibration
This paper contributes to the definition of design clauses for coarse recycled aggregate concrete. One of the main reasons for scepticism towards recycled aggregate concrete is the...
Self-healing evaluation of bacteria grouted light weight aggregate concrete containing rice husk ash and steel fibers
Self-healing evaluation of bacteria grouted light weight aggregate concrete containing rice husk ash and steel fibers
Utilization of microbiologically induced calcite precipitation along with fiber composite have great influence on improving strength and durable properties of concrete. The concept...
Development of hybrid SVM-FA, DT-FA and MLR-FA models to predict the flexural strength (FS) of recycled concrete
Development of hybrid SVM-FA, DT-FA and MLR-FA models to predict the flexural strength (FS) of recycled concrete
Recycled concrete from construction waste used as road material is a current sustainable approach. To provide feasible suggestions for civil engineers to prepare recycled concrete ...
Investigating the Effect of Steel Wire and Carbon Black from Worn Out Tyre on the Strength of Concrete
Investigating the Effect of Steel Wire and Carbon Black from Worn Out Tyre on the Strength of Concrete
Technology in concrete is rapidly developing to improve the quality and properties of concrete. One of the many recycled materials is worn-out tyres. Currently, the use of tires is...