Understanding the wear behavior of various railroad steels used in different components such as rails, wheels, crossings, and curves has a direct impact on the performance of the rail-wheel system in railroad technology. In the present investigation, the wear behavior of steels having varying microstructures (pearlite, ferrite-pearlite, austenite, and bainite) and different chemical compositions has been studied, utilizing a ball-on-disk sliding tribometer under prototypic load and dry conditions. Results indicate that the wear performance of the steel and the mechanism responsible for its wear are significantly governed by the microstructure as well as changes that occur in the contact region during sliding. The formation of tribo-particles comprising oxides of Fe and their possible smearing resulted in high wear resistance in pearlitic steels with considerable plastic deformation of ferrite lamellae compared with austenitic and bainitic steels. In the case of bainitic steel, the absence of any significant smearing of oxide debris, combined with the presence of some distributed tungsten from the ball, contributed to severe wear. On the other hand, in the case of austenitic steel, third-body abrasion by debris particles, comprising a mix of hard metallic and oxide particles, contributed to severe wear despite its high work-hardening ability. On the whole, the pearlitic steel exhibited superior wear resistance with a lower friction coefficient compared with the bainitic and austenitic steels.
Title: Comparative Study on Dry Sliding Wear Behavior of Various Railroad Steels
Description:
Understanding the wear behavior of various railroad steels used in different components such as rails, wheels, crossings, and curves has a direct impact on the performance of the rail-wheel system in railroad technology.
In the present investigation, the wear behavior of steels having varying microstructures (pearlite, ferrite-pearlite, austenite, and bainite) and different chemical compositions has been studied, utilizing a ball-on-disk sliding tribometer under prototypic load and dry conditions.
Results indicate that the wear performance of the steel and the mechanism responsible for its wear are significantly governed by the microstructure as well as changes that occur in the contact region during sliding.
The formation of tribo-particles comprising oxides of Fe and their possible smearing resulted in high wear resistance in pearlitic steels with considerable plastic deformation of ferrite lamellae compared with austenitic and bainitic steels.
In the case of bainitic steel, the absence of any significant smearing of oxide debris, combined with the presence of some distributed tungsten from the ball, contributed to severe wear.
On the other hand, in the case of austenitic steel, third-body abrasion by debris particles, comprising a mix of hard metallic and oxide particles, contributed to severe wear despite its high work-hardening ability.
On the whole, the pearlitic steel exhibited superior wear resistance with a lower friction coefficient compared with the bainitic and austenitic steels.
Related Results
Multi-response optimization of tribological characteristics of aluminum MMCs using PCA
Multi-response optimization of tribological characteristics of aluminum MMCs using PCA
Purpose
– Since, wear is the one of the most commonly encountered industrial problems leading to frequent replacement of components there is a need to develop metal...
Primerjalna književnost na prelomu tisočletja
Primerjalna književnost na prelomu tisočletja
In a comprehensive and at times critical manner, this volume seeks to shed light on the development of events in Western (i.e., European and North American) comparative literature ...
Retained Austenite in Bainitic Steels
Retained Austenite in Bainitic Steels
Bainite is formed through the transformation of austenite, and a portion of the austenite remains untransformed within the bainitic microstructure as retained austenite. The perfor...
Dry sliding wear behavior of Saffil fiber-reinforced Mg-10Gd-3Y-0.5Zr magnesium alloy-based composites
Dry sliding wear behavior of Saffil fiber-reinforced Mg-10Gd-3Y-0.5Zr magnesium alloy-based composites
Dry sliding wear behavior of the creep-resistant magnesium alloy Mg-10Gd-3Y-0.5Zr and its composites have been investigated in this study. Magnesium matrix composites are prepared ...
Characteristic Aspects of Metal Wear: Wear-Induced Wear Transition and Characteristics of Wear Track Profiles
Characteristic Aspects of Metal Wear: Wear-Induced Wear Transition and Characteristics of Wear Track Profiles
This chapter describes two characteristic phenomena of metal wear that are usually not often considered but are related to the basic aspects of wear. The first is a mild-to-severe ...
Effects of different factors on the friction and wear mechanical properties of titanium alloy materials with cortical bones at near service conditions
Effects of different factors on the friction and wear mechanical properties of titanium alloy materials with cortical bones at near service conditions
Abstract
Artificial joint is one of the most effective methods to treat joint injuries. The service performance of artificial joints is gradually bad due to the wear of art...
Impact of coating and microstructure on wear resistance of tool steels for wood cutting: a novel approach to quantification and analysis of wear-related damages
Impact of coating and microstructure on wear resistance of tool steels for wood cutting: a novel approach to quantification and analysis of wear-related damages
AbstractSquaring, a wood transformation process, is an operation which consists of introducing the logs into a squaring machine which then uses sharp tools to cut the wood into pie...
Comparison of Abrasive Wear Resistance of Hardox Steel and Hadfield Cast Steel
Comparison of Abrasive Wear Resistance of Hardox Steel and Hadfield Cast Steel
Among the materials used for components subjected to abrasive wear, chromium cast iron, hardfaced layers, martensitic steels and Hadfield steel should be singled out. Each of these...