The Cracking Mechanism of Ferritic-Austenitic Cast Steel
View through CrossRef
Abstract
In the high-alloy, ferritic - austenitic (duplex) stainless steels high tendency to cracking, mainly hot-is induced by micro segregation processes and change of crystallization mechanism in its final stage. The article is a continuation of the problems presented in earlier papers [1 - 4]. In the range of high temperature cracking appear one mechanism a decohesion - intergranular however, depending on the chemical composition of the steel, various structural factors decide of the occurrence of hot cracking. The low-carbon and low-alloy cast steel casting hot cracking cause are type II sulphide, in high carbon tool cast steel secondary cementite mesh and / or ledeburite segregated at the grain solidified grains boundaries, in the case of Hadfield steel phosphorus - carbide eutectic, which carrier is iron-manganese and low solubility of phosphorus in high manganese matrix. In duplex cast steel the additional factor increasing the risk of cracking it is very “rich” chemical composition and related with it processes of precipitation of many secondary phases.
Title: The Cracking Mechanism of Ferritic-Austenitic Cast Steel
Description:
Abstract
In the high-alloy, ferritic - austenitic (duplex) stainless steels high tendency to cracking, mainly hot-is induced by micro segregation processes and change of crystallization mechanism in its final stage.
The article is a continuation of the problems presented in earlier papers [1 - 4].
In the range of high temperature cracking appear one mechanism a decohesion - intergranular however, depending on the chemical composition of the steel, various structural factors decide of the occurrence of hot cracking.
The low-carbon and low-alloy cast steel casting hot cracking cause are type II sulphide, in high carbon tool cast steel secondary cementite mesh and / or ledeburite segregated at the grain solidified grains boundaries, in the case of Hadfield steel phosphorus - carbide eutectic, which carrier is iron-manganese and low solubility of phosphorus in high manganese matrix.
In duplex cast steel the additional factor increasing the risk of cracking it is very “rich” chemical composition and related with it processes of precipitation of many secondary phases.
Related Results
Unveiling the third dimension of glass
Unveiling the third dimension of glass
Glass as a material has always fascinated architects. Its inherent transparency has given us the ability to create diaphanous barriers between the interior and the exterior that al...
Sulfide Stress-Cracking Resistance of Nitrogen-Strengthened Stainless Steels
Sulfide Stress-Cracking Resistance of Nitrogen-Strengthened Stainless Steels
Summary
Although most materials used in oilfield operations are carbon steel or alloy steel, stainless alloys are used in critical areas where salt water, CO2, an...
Sulfide Stress Cracking Resistance Of Nitrogen-Strengthened Stainless Steels
Sulfide Stress Cracking Resistance Of Nitrogen-Strengthened Stainless Steels
Abstract
Although the bulk of the materials used in oil field operations are carbon steel or alloy steel, stainless alloys are employed in critical areas where sa...
Stainless Steels
Stainless Steels
AbstractStainless steels are those alloys of iron and chromium, with or without other elements, containing at least 11% chromium. There are six basic classifications of stainless s...
Management of Distal 1/3rd Closed Forearm Fractures in Children above Elbow Plaster Cast versus Below Elbow Plaster Cast
Management of Distal 1/3rd Closed Forearm Fractures in Children above Elbow Plaster Cast versus Below Elbow Plaster Cast
Objective: To determine if below-elbow casts are as effective as above-elbow casts in the treatment of the distal third closed forearm fractures in children.
Materials and Me...
Evaluating the Flaw Tolerance and Ductile Tearing Resistance of Austenitic Stainless Steel Welds
Evaluating the Flaw Tolerance and Ductile Tearing Resistance of Austenitic Stainless Steel Welds
Abstract
In general, austenitic stainless steels behave in a more ductile than brittle manner and do not typically experience a ductile-to-brittle transition like ty...
Numerical Simulation of Hot Cracking Tests
Numerical Simulation of Hot Cracking Tests
One of the main nuclear materials is the austenitic stainless steels, which have good ductility and toughness, high thermal expansion coefficients and a thermal conductivity lower ...
Possibility of Zinc Embrittlement in Fire
Possibility of Zinc Embrittlement in Fire
ABSTRACT
Zinc embrittlement is known as a kind of liquid metal embrittlement, a phenomenon where austenitic stainless steel and nickel alloy becomes brittle and/or c...