EFFECT OF DIFFERENT SALIVA DECONTAMINATION PROCEDURES ON THE SHEAR BOND STRENGTH OF A UNIVERSAL EIGHTH GENERATION ADHESIVE SYSTEM TO DENTIN AFTER POLYMERIZATION - AN IN VITRO STUDY
View through CrossRef
Aim: To evaluate and compare the effect of saliva decontamination procedure on the shear bond strength of a Universal eighth generation adhesive system to dentin after polymerization. Materials & Method: Forty extracted non-carious premolars were mounted on a acrylic block and their occlusal surfaces were grounded flat to exposed the middle depth dentin. The teeth were then randomly divided into five Groups: Group A(control), Group B(Bonding, Saliva, Air-dried), Group C(Bonding, Saliva, Air-dried, Rinse), Group D(Bonding, Saliva, Air-dried, Re-bonding) & Group E (Bonding, Saliva, Air-dried, Rinse, Re-bonding). A teflon tube of 2x3 mm dimension was used to pack composite on the treated dentin surface and light cured for 40s. Shear Bond strength was then measured using instron testing machine at a crosshead speed of 1mm/min. Data were statistically analysed using ONE WAY-ANOVA and TUKEYS test. Result: It was observed that, the highest mean shear bond strength was found in Group D(Bonding, Saliva, Air-dried, Re-bonding) & Group E(Bonding, Saliva, Air-dried, Rinse, Re-bonding) with a mean value of 23.87 each. The least mean value was seen in Group C(Bonding, Saliva, Air-dried, Rinse), 13.25. When an intergroup comparision was made, statistically significant difference was seen between the various groups except Group A(control)-Group D(Bonding, Saliva, Air-dried, Re-bonding)-Group E(Bonding, Saliva, Air-dried, Rinse, Re-bonding) and Group B(Bonding, Saliva, Air-dried)-Group C(Bonding, Saliva, Air-dried, Rinse). Conclusion: Salivary contamination significantly decreases the bond strength of the adhesive to dentin after polymerization. Rinsing and Air-drying of the cured contaminated dentin surface was not sufficient to restore the shear bond strength. However reapplication of adhesive system after rinsing and air-drying of the cured contaminated dentin surface fully restored the bond strength.
International Journal Of Advanced Research
Title: EFFECT OF DIFFERENT SALIVA DECONTAMINATION PROCEDURES ON THE SHEAR BOND STRENGTH OF A UNIVERSAL EIGHTH GENERATION ADHESIVE SYSTEM TO DENTIN AFTER POLYMERIZATION - AN IN VITRO STUDY
Description:
Aim: To evaluate and compare the effect of saliva decontamination procedure on the shear bond strength of a Universal eighth generation adhesive system to dentin after polymerization.
Materials & Method: Forty extracted non-carious premolars were mounted on a acrylic block and their occlusal surfaces were grounded flat to exposed the middle depth dentin.
The teeth were then randomly divided into five Groups: Group A(control), Group B(Bonding, Saliva, Air-dried), Group C(Bonding, Saliva, Air-dried, Rinse), Group D(Bonding, Saliva, Air-dried, Re-bonding) & Group E (Bonding, Saliva, Air-dried, Rinse, Re-bonding).
A teflon tube of 2x3 mm dimension was used to pack composite on the treated dentin surface and light cured for 40s.
Shear Bond strength was then measured using instron testing machine at a crosshead speed of 1mm/min.
Data were statistically analysed using ONE WAY-ANOVA and TUKEYS test.
Result: It was observed that, the highest mean shear bond strength was found in Group D(Bonding, Saliva, Air-dried, Re-bonding) & Group E(Bonding, Saliva, Air-dried, Rinse, Re-bonding) with a mean value of 23.
87 each.
The least mean value was seen in Group C(Bonding, Saliva, Air-dried, Rinse), 13.
25.
When an intergroup comparision was made, statistically significant difference was seen between the various groups except Group A(control)-Group D(Bonding, Saliva, Air-dried, Re-bonding)-Group E(Bonding, Saliva, Air-dried, Rinse, Re-bonding) and Group B(Bonding, Saliva, Air-dried)-Group C(Bonding, Saliva, Air-dried, Rinse).
Conclusion: Salivary contamination significantly decreases the bond strength of the adhesive to dentin after polymerization.
Rinsing and Air-drying of the cured contaminated dentin surface was not sufficient to restore the shear bond strength.
However reapplication of adhesive system after rinsing and air-drying of the cured contaminated dentin surface fully restored the bond strength.
Related Results
Evaluation of Four Different Adhesive Systems’ Bonding Strength Between Superficial and Deep Dentin
Evaluation of Four Different Adhesive Systems’ Bonding Strength Between Superficial and Deep Dentin
The success of adhesive restorations largely depends on the optimal bond strength between the tooth structure and the restorative material. The aim of this study was to evaluate th...
Effect of delayed composite placement over cured adhesive on the dentin shear bond strength of two universal adhesives: an in vitro comparative study
Effect of delayed composite placement over cured adhesive on the dentin shear bond strength of two universal adhesives: an in vitro comparative study
Background and objective. Unconsumed acidic monomers of universal adhesives have issues in the case when utilized with composite resin materials that contain tertiary amine as a co...
Effect of substrate and adhesive system type on composite resin restorations
Effect of substrate and adhesive system type on composite resin restorations
Although it is possible to obtain a reliable bond between enamel and composite resin, the ideal bonding method of composite resin to dentin still needs to be developed. Variables s...
Effect of Different Disinfection Protocols on The Resin Bond Strength to Dentin: In Vitro Study.
Effect of Different Disinfection Protocols on The Resin Bond Strength to Dentin: In Vitro Study.
Abstract
Antimicrobial photodynamic therapy (aPDT) can be adopted as a modality for bacterial decontamination before cavity restoration to decrease the risk of secondary ca...
Improvement of seismic performance of ordinary reinforced partially grouted concrete masonry shear walls
Improvement of seismic performance of ordinary reinforced partially grouted concrete masonry shear walls
Reinforced masonry constitutes about 10% of all low-rise construction in the US. Most of these structures are commercial and school buildings. It may also be used for multi-story h...
Shear bond strength and ultrastructural interface analysis of different adhesive systems to bleached dentin
Shear bond strength and ultrastructural interface analysis of different adhesive systems to bleached dentin
AbstractBackground: It remains unclear as to whether or not dental bleaching affects the bond strength of dentin/resin restoration. Purpose: To evaluated the bond strength of adhes...
Bond strength of self-adhesive resin cements to deep dentin
Bond strength of self-adhesive resin cements to deep dentin
Introduction and objective: Self-adhesive resin cements are applied in only one clinical step whose technique is considered less sensitive and of easy handling. However, there is s...
Pengaruh air kelapa terhadap peningkatan pH saliva
Pengaruh air kelapa terhadap peningkatan pH saliva
Abstract: Dental caries is a disease that attacks the hard tooth tissue. One of the causes of dental caries is the acidogenic bacteria. The bacterial growth is influenced by the co...